Hi folks

I finally started on my first frame (HT-DT lug brazed yesterday) and it went well as far as I can tell. Bronze brazing.

I do anticipate making a mistake at some point though, and feeling the need to reheat a joint to correct a flow issue or tidy a shoreline.

Tubing is standard cromo with 0.9-0.6-0.9 walls.

How many times would I be able to safely heat a joint with that basic tubing? One re-heat? No re-heats?

Would like to know in advance before I do something silly in the heat (.... sorry) of the moment.

Thank you,

Colin Tuff