I'm dropping in some stainless dropouts into CroMo stays and would love a bit of guidance on which filler to use. I usually keep Gasflux 50% around for bosses. But I'm wondering if I should opt for 45% or even the 38% to fill the inside of the dropout.


I have some nickel-silver rod laying around but every time I use it I feel like I'm brazing with boogers.